On Sun, 26 Oct 1997, you wrote:

> The standard job seems to be beadblast everything, clean the
> rocker shaft, grind shallow oil reliefs in the shaft, then hard-chrome
> that piece,

But do they handle worn rocker shafts - the chrome surely can't fill the 
void left by average wear.

> re-radius
> the rocker noses

How does that affect the case hardening? Wouldn't average rocker nose 
wear go through the hardened layer?