To: | Davesmbox@aol.com, datsun-roadsters@autox.team.net |
---|---|
Subject: | Re: Mag testing a head |
From: | RWM <RWM@rwmann.com> |
Date: | Fri, 05 Aug 2005 14:41:23 -0400 |
I suspect he equates magnafluxing of a ferrous part with dye penetrant testing of a non-ferrous part, which is of course, quite different, but still NDT. - Bob Mann, '68 2000 Solex; no dye, no flux Davesmbox@aol.com wrote: >There is a 2000 head on ebay. I don't need another one but I was currious. >The seller says it was Mag tested for cracks. How do you mag an aluminum head? >I know how they do a steel one. Is there a way or has this guy been snorting >his iron filings? > >Dave |